Material Drying 8 visualizaciones

Product dimensions out of tolerance range

Fenómeno del problema
Product dimensions out of tolerance range, too large or too small, dimensions unstable, fluctuating with batch or time
Análisis de la causa
Mold dimension design did not consider cellulose acetate butyrate shrinkage 0.4-0.6% Unstable injection conditions (pressure/temperature fluctuation) Raw material moisture variation causing shrinkage differences Cellulose acetate butyrate dimensional change after moisture absorption (especially obvious for PA types) Insufficient cooling time, product demolded before fully shrunk
Solución
Precisely design mold dimensions according to 0.4-0.6% shrinkage Stabilize injection conditions, control temperature and pressure fluctuation Strictly control raw material moisture Cellulose acetate butyrate is highly hygroscopic and needs conditioning treatment to stabilize dimensions Extend cooling time to ensure full shrinkage
Conclusión clave
Dimension out of tolerance requires stable process conditions and moisture control
dimension out of toleranceshrinkagemoistureprocess stability