Material Drying 8 visualizaciones

Product color inconsistent with the standard color plate

Fenómeno del problema
Product color inconsistent with the standard color plate, locally or entirely yellowish and dark, transparency decreased for transparent products
Análisis de la causa
Barrel temperature too high causing cellulose acetate butyrate thermal degradation and discoloration Drying temperature too high or time too long, oxidative discoloration Screw shear too intense, local degradation Regrind used multiple times, degradation accumulation discoloration Uneven dispersion of pigment or color masterbatch
Solución
Lower barrel temperature to the low range of 170-230°C Strictly control drying conditions 75-85°C/3-4h to avoid over-drying Reduce screw speed to reduce shear Limit regrind ratio ≤15% Improve color masterbatch dispersion, add mixing section
Conclusión clave
Color difference needs to be addressed from temperature, shear, drying and regrind control
color differenceyellowingthermal degradationdispersion