Injection Molding 7 visualizaciones

Thin-wall products with wall thickness <1mm have many short shot, warpage and deformation problems

Fenómeno del problema
Thin-wall products with wall thickness <1mm have many short shot, warpage and deformation problems
Análisis de la causa
Thin-wall filling difficult, melt front rapidly condenses, short shot Injection speed needs to be extremely fast, thin-wall condensation time short Gate design needs to ensure filling of thin-wall areas Holding time short, gate rapidly freezes, insufficient shrinkage compensation Cellulose acetate butyrate flowability needs to meet thin-wall requirements
Solución
Increase injection speed to ensure fast thin-wall filling Use multi-point gates to ensure filling of thin-wall areas Raise mold temperature to the high side of 40-80°C to delay condensation Increase holding pressure to compensate for rapid thin-wall gate freezing Select high-flowability cellulose acetate butyrate variety
Conclusión clave
Thin wall requires high-speed injection and high-flowability material
thin-wall injectionhigh-speed fillingflowabilitycellulose acetate butyrate