Material Drying 8 visualizaciones

Product surface has no gloss

Fenómeno del problema
The product surface has no gloss, appears matte or dull, and the gloss differs greatly from the standard sample
Análisis de la causa
The mold cavity surface is rough, insufficient polishing The mold temperature is low (below 40-80°C), the melt front cools quickly and cannot replicate the mold surface The injection speed is too slow, the melt contact time with the mold is insufficient The raw material contains moisture, affecting surface quality The barrel temperature is low, melt fluidity insufficient
Solución
Polish the mold cavity to mirror level Increase the mold temperature to the higher value of 40-80°C Appropriately increase the injection speed Fully dry the raw material Appropriately increase the barrel temperature to the higher value of 170-230°C
Conclusión clave
Surface gloss requires improving the mold surface and increasing the mold temperature
poor glossmold temperaturemold polishinginjection speed