Processing Machinery 8 visualizaciones

Insufficient Mixing of CMC

Fenómeno del problema
After blending CMC with fillers/additives, dispersion is uneven with local agglomeration
Análisis de la causa
Screw mixing section length is insufficient; number of kneading blocks is not enough; improper feeding method means additives and CMC are not fully contacted
Solución
1)Increase screw mixing section length to 3-4D; 2)Increase the number of kneading blocks; 3)Add additives after the side feeding port to increase mixing time
Conclusión clave
Insufficient mixing is caused by improper screw design; increasing the mixing section is the key
CMCinsufficient mixingscrew mixing sectionkneading blocksside feeding