Processing Machinery 8 visualizaciones

Poor Plasticization of CMC

Fenómeno del problema
Unmelted particles appear in CMC products, plasticization is incomplete
Análisis de la causa
Screw compression ratio is insufficient <2.5 and plasticizing pressure is low; screw speed is low and shear is insufficient; processing temperature is low
Solución
1)Select a screw with compression ratio >3; 2)Increase screw speed to increase shear; 3)Increase processing temperature by 5-10°C
Conclusión clave
Poor plasticization is caused by improper screw design; optimizing the screw and increasing temperature are the key
CMCpoor plasticizationscrew compression ratioshear rateprocessing temperature