Material Analysis 16 visualizaciones

DSTDP product dimensional change during long-term storage

Fenómeno del problema
DSTDP product dimensions change ±2-3% after 3 months of storage, exceeding the ±0.5% requirement
Análisis de la causa
DSTDP physical aging relaxation causes continuous dimensional change; secondary crystallization slowly changes density and dimensions; slow migration of low-molecular substances changes local density
Solución
1) Anneal products at 80°C/4h before leaving the factory to stabilize dimensions; 2) select high molecular weight grades to reduce low-molecular substances; 3) slight crosslinking to reduce molecular chain mobility and inhibit aging; 4) control storage environment temperature at 23±2°C to reduce the influence of temperature change
Conclusión clave
Dimensional change is caused by physical aging; annealing treatment and slight crosslinking are the measures to stabilize dimensions
DSTDP dimensional stabilityphysical agingannealingsecondary crystallizationslight crosslinking