Processing Machinery 8 visualizaciones

DSTDP material changeover residue

Fenómeno del problema
After DSTDP material changeover, the first 5-10 products contain previous material residue, color difference and performance deviation
Análisis de la causa
Large amount of previous material residue in the barrel and screw; incomplete cleaning, residue in dead corner zones; insufficient purging compound amount
Solución
1) Increase purging compound amount to 2-3 times the barrel capacity; 2) increase speed and temperature during cleaning to accelerate removal; 3) disassemble the screw to thoroughly clean dead corners
Conclusión clave
Material changeover residue is caused by incomplete cleaning; thorough cleaning and disassembly are key
DSTDPmaterial changeover residuepurging compoundscrew disassemblydead corner cleaning

¿Le ha resultado útil?

0 personas encontraron esto útil

ChemAI