Fenómeno del problema
DSTDP product tensile strength 15-20% below the standard value
Análisis de la causa
DSTDP molecular weight on the low side, strength foundation insufficient; filler interface poor, not playing a reinforcing role; excessive orientation, strong longitudinally and weak transversely
Solución
1) Select high molecular weight DSTDP grades; 2) filler coupling agent treatment to improve interface; 3) reduce orientation to reduce longitudinal-transverse difference
Conclusión clave
Insufficient tensile strength is caused by molecular weight and poor interface; selecting high MW grades is key