Material Analysis 15 visualizaciones

Glass Fibre hardness too high

Fenómeno del problema
Glass Fibre product Shore hardness 5-10 degrees higher than target, feels hard
Análisis de la causa
Glass Fibre crystallinity too high, rigidity increased; filler added too much; cooling too fast, crystallization imperfect but rigidity frozen
Solución
1) Reduce cooling rate to make crystallization complete and reduce hard feel; 2) reduce filler addition; 3) add plasticizer 0.5wt% to reduce hardness
Conclusión clave
High hardness is caused by crystallization and filler; adjusting cooling and filler is key
Glass Fibrehigh hardnesscrystallinityfiller amountplasticizer