Injection Molding 2 visualizaciones

MP '2079851475616104452 cold slug marks

Fenómeno del problema
MP injection molded products show cold slug marks near the gate
Análisis de la causa
nozzle temperature low causing previous injection residue to cool and solidify in the nozzle; cold slug well design insufficient, cannot hold the cold slug; injection pressure insufficient
Solución
1) raise nozzle temperature to 150-170°C; 2) design the mold with a sufficiently large cold slug well; 3) ensure fresh melt at the nozzle front before each injection; 4) raise injection pressure to push the cold slug through the gate
Conclusión clave
cold slug marks are caused by solidified residue in the nozzle; raising nozzle temperature and cold slug well design are key
MP injection cold slug mark nozzle temperature cold slug well injection pressure