Processing Machinery
8 visualizaciones
MP material changeover residue
Fenómeno del problema
after MP material changeover, the first 5-10 products contain previous material residue, color difference and property deviation
Análisis de la causa
large amount of previous material residue in the barrel and screw; incomplete cleaning, residue in dead zones; insufficient purging material amount
Solución
1) increase purging material to 2-3 times the barrel capacity; 2) increase rotation speed and temperature during cleaning to accelerate removal; 3) disassemble the screw to thoroughly clean dead zones
Conclusión clave
changeover residue is caused by incomplete cleaning; thorough cleaning and disassembly are key