Injection Molding 7 visualizaciones

MP surface tiger-skin pattern

Fenómeno del problema
MP injection molded product surface has tiger-skin pattern, alternating light-dark streaks, width 2-5mm
Análisis de la causa
injection speed unstable, melt front fluctuates fast and slow; mold temperature low <30°C, front rapidly cools
Solución
1) multi-stage injection slow-fast-slow to stabilize the front; 2) raise mold temperature to 40-50°C; 3) increase injection pressure to stabilize advancement
Conclusión clave
tiger-skin pattern is caused by unstable injection front; multi-stage injection and high mold temperature are key
MP tiger-skin pattern injection speed multi-stage injection mold temperature control