Injection Molding 8 visualizaciones

Optimization of the degradation problem of PBD in '2079851475616104452

Fenómeno del problema
Polybutadiene PBD, as an elastomer toughening modifier or HIPS component, exhibited degradation-related abnormalities during the '2079851475616104452 process.
Análisis de la causa
The gel content of PBD affects processing; improper crosslinking control leads to performance deterioration.
Solución
According to application requirements, control crosslinking density to systematically solve the problem.
Conclusión clave
The core of PBD processing lies in thermal-oxidative protection.
PBDpolybutadieneHIPS