Material Analysis 15 visualizaciones

Analysis and solution of bubble of High-temp MB in PA industrial parts

Fenómeno del problema
High-temp MB shows abnormal performance related to bubble when producing industrial parts with PA.
Análisis de la causa
The main cause is parameters deviating from the window in terms of bubble leading to unstable processing.
Solución
Comprehensively solve the bubble problem from the perspective of formulation optimization.
Conclusión clave
Control of bubble of High-temp MB is the key link to ensure processing quality.
high-temperature resistant masterbatchbubblePAindustrial parts