Material Drying 8 visualizaciones

Control of transparency abnormality in PEOX hot pressing textiles

Fenómeno del problema
During PEOX hot pressing production of textiles, the problem of uneven transparency occurs.
Análisis de la causa
Mainly due to the processing temperature deviating from the window +60-100°C, moisture content >0.5% exceeding the standard, and excessively long residence time.
Solución
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
Conclusión clave
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.