Material Analysis
3 visualizaciones
Regulation of die buildup of PPA in BOPP Processing
Fenómeno del problema
The die buildup abnormality of the PPA processing aid in BOPP production affects output.
Análisis de la causa
The die buildup of the PPA fluoropolymer is unsatisfactory at an addition amount of 0.03%, and the molecular weight needs to be optimized.
Solución
Adjust the PPA pretreatment process combined with formulation adjustment.
Conclusión clave
The key to the performance of PPA lies in uniform dispersion.
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!