Material Analysis 8 visualizaciones

Analysis and Resolution of addition ratio of Smooth MB in heat shrink film label film

Fenómeno del problema
When Smooth MB produces label film with heat shrink film, abnormal performance related to addition ratio occurs.
Análisis de la causa
The main cause is lax control of parameters in the aspect of addition ratio, leading to processing instability.
Solución
Comprehensively resolve the addition ratio problem from the perspective of process adjustment.
Conclusión clave
The control of addition ratio of Smooth MB is the key link in ensuring processing quality.