Material Analysis
8 visualizaciones
Analysis and Resolution of heat sealability of Smooth MB in heat shrink film composite film
Fenómeno del problema
When Smooth MB produces composite film with heat shrink film, abnormal performance related to heat sealability occurs.
Análisis de la causa
The main cause is lax control of parameters in the aspect of heat sealability, leading to processing instability.
Solución
Comprehensively resolve the heat sealability problem from the perspective of formulation optimization.
Conclusión clave
The control of heat sealability of Smooth MB is the key link in ensuring processing quality.