POE tensile strength insufficient
Fenómeno del problema
POE product tensile strength 15-20% below standard value
Análisis de la causa
POE molecular weight low, strength foundation insufficient; filler interface poor, no reinforcing effect; excessive orientation, longitudinal strong and transverse weak
Solución
1) Select high molecular weight POE grade; 2) Filler coupling agent treatment to improve interface; 3) Reduce orientation to reduce longitudinal-transverse difference
Conclusión clave
Insufficient tensile strength is caused by molecular weight and poor interface; selecting high MW grade is key