Burnt yellow spots on injection molded products
Fenómeno del problema
Yellow-brown burnt spots appear locally on the product, accompanied by an odor
Análisis de la causa
>260C local overheating causes material decomposition in dead corners, producing HF
Solución
Lower the temperature, check temperature control elements, reduce dead corners, and reduce the injection speed
Conclusión clave
Thermal decomposition produces HF and must be strictly avoided