Fenómeno del problema
Unreasonable temperature settings of each barrel section lead to poor plasticization or local degradation.
Análisis de la causa
The temperature of each section is not set in a decreasing manner according to the characteristics of PBT; the temperature difference between sections is too large or too small.
Solución
Adopt the recommended temperature control curve: feeding section 220-230°C, compression section 240-250°C, metering section 250-260°C.
Conclusión clave
PBT section temperature control is the basis of precision '2079851475616104452.