Material Drying 6 visualizaciones

Sticking of PET during drying

Fenómeno del problema
PET pellets stick and agglomerate in the dehumidifying dryer, cannot discharge normally.
Análisis de la causa
Drying temperature set too high (exceeding PET softening point), temperature control system failure, material stays too long in high-temperature zone, amorphous PET low softening.
Solución
Strictly control drying temperature ≤175°C; calibrate temperature control; avoid long residence (>8h); pre-crystallize amorphous PET first.
Conclusión clave
PET drying sticking requires strict control of temperature and residence time.
PETdryingstickingpre-crystallizationtemperature control