Injection Molding 15 visualizaciones

Insufficient weld line strength of PET injection molded parts

Fenómeno del problema
The strength at the weld line of PET injection molded products is significantly lower than the bulk, and the product breaks along the weld line in impact testing.
Análisis de la causa
The two melt fronts fail to fully fuse (temperature on the low side); molecular chain orientation at the weld line is unfavorable for strength; venting is poor.
Solución
Increase melt temperature and mold temperature; increase injection speed and holding pressure; optimize gate position; improve venting at the weld line.
Conclusión clave
PET weld line strength needs to be comprehensively improved through temperature, pressure and gate layout.
PETweld lineinsufficient strengthmolecular chain orientationventing