Material Drying
7 visualizaciones
Fogging on the surface of PET parts after packaging
Fenómeno del problema
After transparent PET packaging products are sealed and packaged, the inner surface fogs up and transparency decreases.
Análisis de la causa
Moisture in the environment condenses on the PET surface (large temperature difference inside and outside the packaging produces condensation); the PET surface is hydrophilic.
Solución
Fully cool to room temperature before packaging; use anti-fog additives to treat the surface; control the temperature and humidity of the packaging environment.
Conclusión clave
PET surface fogging affects display effect and needs anti-fog treatment.
¿Le ha resultado útil?
0 personas encontraron esto útil