PETG injection molded product haze due to mold release agent residue
Fenómeno del problema
After using mold release agent, the PETG product surface becomes hazy, and transparency and gloss decrease.
Análisis de la causa
Mold release agent sprayed excessively or unevenly distributed, remaining on the product surface, the release agent reacts with and erodes PETG.
Solución
Reduce mold release agent dosage with precision spraying; select a dedicated transparent plastic release agent; minimize dependence through mold treatment.
Conclusión clave
PETG transparent products should minimize the use of mold release agent.