Injection Molding
8 visualizaciones
Selection of mold temperature controller for PLA '2079851475616104452
Fenómeno del problema
For crystalline PLA, a high-temperature grade mold temperature controller (>100°C) needs to be selected.
Análisis de la causa
Conventional water temperature controllers (maximum 95°C) cannot meet the PLA crystallization mold temperature requirements.
Solución
Retrofit an oil temperature controller (up to 180°C) to achieve the crystallization temperature of 120°C.
Conclusión clave
PLA '2079851475616104452 equipment configuration needs to consider the high mold temperature demand.