Injection Molding
8 visualizaciones
Odor residue in products during PLA '2079851475616104452
Fenómeno del problema
PLA products have residual lactic acid or sweet smell.
Análisis de la causa
Low molecular lactic acid produced by degradation remains, the processing temperature is too high, and monomers remain in the raw material.
Solución
Control the processing temperature <200°C; fully ventilate; ventilate and air after demolding.
Conclusión clave
The odor of PLA products affects the use experience.
¿Le ha resultado útil?
0 personas encontraron esto útil