Fenómeno del problema
When the back pressure is insufficient, PLA plasticization is incomplete.
Análisis de la causa
The viscosity of PLA is high, and a certain back pressure is required to ensure plasticization and mixing.
Solución
Set the back pressure at 0.5-1.5MPa; observe the melt temperature and plasticization quality.
Conclusión clave
The PLA back pressure needs to match the melt characteristics.