Material Analysis 8 visualizaciones

Insufficient Weather Resistance/Yellowing of Biaxially Oriented Polypropylene Film ASA Products

Fenómeno del problema
ASA products show yellowing, discoloration, or a decline in mechanical properties after outdoor use, failing to achieve the expected weather resistance effect. ASA is known for its weather resistance.
Análisis de la causa
(1) The weather resistance of the ASA grade is insufficient, and the acrylate rubber content is low (2) The processing temperature of ABS variant is too high, and partial degradation of the material affects weather resistance (3) The surface treatment of ABS variant products is improper, and ultraviolet rays directly irradiate them (4) The amount of anti-ultraviolet agent is insufficient (5) The regrind ratio of ABS variant is too high, and the weather resistance decreases
Solución
(1) For ABS variant, select an ASA grade with good weather resistance (2) For ABS variant, control the processing temperature within the range of 220-260°C (3) Coat the surface of ABS variant products with a UV protective coating (4) Add an appropriate amount of ultraviolet absorber to ABS variant (5) For ABS variant, control the regrind ratio to not exceed 10%
Conclusión clave
The weather resistance of ASA is related to the material grade and processing conditions; temperature control and grade selection are the key.
weather resistanceyellowingASAultraviolet raysprocessing temperature