Processing Machinery 8 visualizaciones

Poor thermal stability of transparent ABS (methyl methacrylate-acrylonitrile-butadiene-styrene copolymer) during processing

Fenómeno del problema
Transparent ABS (methyl methacrylate-acrylonitrile-butadiene-styrene copolymer) has poor thermal stability during processing; performance decreases significantly after repeated processing, with severe degradation
Análisis de la causa
Insufficient antioxidant addition or improper type Processing temperature too high (exceeding the 210-250°C upper limit) accelerates degradation Excessive screw shear accelerates thermo-oxidative degradation Regrind ratio too high, degradation accumulates Antioxidants fail at high temperature
Solución
Increase antioxidant addition amount Reduce processing temperature to a reasonable value of 210-250°C Reduce screw rotation speed to reduce shear Reduce regrind ratio ≤15% Select antioxidants with good high-temperature stability
Conclusión clave
Thermal stability needs to start from antioxidants and temperature control
thermal stabilityantioxidantdegradationtemperature

¿Le ha resultado útil?

0 personas encontraron esto útil

ChemAI