Thermoforming 13 visualizaciones

Poor adhesion of electroplating/spray coating on polystyrene products

Fenómeno del problema
After electroplating or spray coating, the coating adhesion is poor, and blistering or peeling easily occurs.
Análisis de la causa
(1) Product surface tension is insufficient, and the coating is difficult to adhere (2) The product surface has release agent or oil stain residues (3) Product internal stress is large, affecting coating adhesion (4) Pretreatment before electroplating/spray coating is insufficient (5) The coating material does not match the substrate
Solución
(1) Perform corona or flame treatment on the product surface (2) Ensure the product surface is clean and free of release agent (3) Reduce product internal stress (annealing treatment) (4) Strengthen pretreatment (degreasing, roughening, etc.) (5) Select matching coating materials
Conclusión clave
Electroplating and spray coating adhesion is determined by surface energy and surface condition.
electroplating adhesionspray coating adhesionsurface tensionsurface treatmentinternal stress