Material Analysis
8 visualizaciones
Pockmarks/pinholes on product surface
Fenómeno del problema
A large number of tiny holes or pits appear on the surface, with rough hand feel, seriously affecting appearance
Análisis de la causa
Dispersed phase particles are too large, forming defects on the product surface; gas entrained during melt filling is not compacted; additive decomposition
Solución
Improve the dispersion shear effect of the screw mixing section; reduce injection speed to reduce gas entrainment; increase holding pressure and extend holding time by 50%
Conclusión clave
Surface pinhole defects originate from insufficient dispersion and gas entrainment
¿Le ha resultado útil?
0 personas encontraron esto útil
¡Gracias por sus comentarios!