Production & Quality 11 visualizaciones

Product toughness greatly reduced at low temperature (below -10°C)

Fenómeno del problema
Products undergo brittle fracture in winter or low-temperature environments
Análisis de la causa
The PP matrix significantly embrittles below its embrittlement temperature (-10~0°C); stress concentration at fiber ends more easily triggers fracture at low temperature; the interface embrittles at low temperature
Solución
Use high-impact copolymer PP as the matrix (PP-B or PP-R); add elastomer toughening (POE, EPDM); reduce glass fiber content or shorten fiber length to reduce stress concentration
Conclusión clave
Low-temperature toughness is the main constraint for LGFPP applications in outdoor and low-temperature environments
low-temperature toughnessembrittlement temperaturecopolymer PPelastomerPOE

¿Le ha resultado útil?

0 personas encontraron esto útil