PEI rapidly re-absorbs moisture after drying
Fenómeno del problema
After passing drying, the moisture content rises back above the standard after 15-30 minutes of exposure to air
Análisis de la causa
PEI absorbs moisture extremely fast (saturated 1.25% water absorption); production workshop ambient humidity too high (>60%RH); no sealed connection between drying and '2079851475616104452
Solución
Use a drying hopper for online continuous feeding; transfer dried material in sealed containers or direct hot material conveying; install a dehumidification system in the workshop to reduce ambient humidity
Conclusión clave
The moisture absorption rate of PEI determines that a full-process moisture protection solution must be used