Extrusion & Post 17 visualizaciones

PES hollow fiber membrane unstable drawing

Fenómeno del problema
Uneven wall thickness or broken filaments occur in hollow fiber membrane spinning
Análisis de la causa
The spinning solution (casting solution) composition does not match; coagulation bath temperature and composition fluctuate; draw ratio set improperly
Solución
Optimize the polymer content and additive formulation of the spinning solution; precisely control the coagulation bath conditions; adjust the draw ratio within a suitable range
Conclusión clave
The PES hollow fiber membrane manufacturing process is high-precision process control
hollow fiber membranespinning solutioncoagulation bathdraw ratio