Q
Excessively fast screw wear of PET '2079851475616104452 machine
A
Reinforced PET processing requires wear-resistant special screws and barrels.
Injection Molding PETglass fiber reinforcementscrew wearbimetallicabrasion
Q
Excessively long PET preform injection cycle
A
The PET preform molding cycle directly affects production costs.
Injection Molding PETmolding cyclecoolingproductivitypreform
Q
Severe internal stress birefringence in PET injection molded parts
Q
Flow marks appearing on PET injection molded parts
A
PET flow marks are caused by an unstable melt front during filling.
Injection Molding PETflow markmelt frontfillingmold temperature
Q
Black spots on PET injection molded products
Q
Poor gloss of PET injection molded products
A
Q
Fluidity decline of PET modified material
Q
Uneven breakage of PET bottle cap tamper-evident rings
A
Uniform breaking of PET bottle cap tamper-evident rings requires fine structural design and material proportioning.
Injection Molding PETbottle captamper-evident ringconnecting bridgeweld line
Q
High residual monomer content in PET '2079851475616104452
A
PET residual monomer control starts from two aspects: raw material selection and processing technology.
Injection Molding PETresidual monomersethylene glycolterephthalic acid
Q
Barrel corrosion of PET '2079851475616104452 machine
A
Flame retardant PET processing needs to be matched with corrosion-resistant equipment.
Injection Molding PETbarrel corrosionflame retardanthalogenacidic gas