Injection Molding 8 visualizaciones

Excessively long PET preform injection cycle

Fenómeno del problema
The PET preform '2079851475616104452 cycle is too long (>25 seconds), and production efficiency is low.
Análisis de la causa
Cooling time is too long (PET crystallization exotherm causes slow cooling); mold cooling efficiency is insufficient; preform walls are too thick.
Solución
Optimize cooling water channels to increase cooling efficiency; appropriately reduce mold temperature; thin the preform wall thickness; use rapid heating and cooling technology.
Conclusión clave
The PET preform molding cycle directly affects production costs.
PETmolding cyclecoolingproductivitypreform