Q
CEF injection molded part has oil spots
Q
CEF injection weld line strength low
Q
CEF injection flow length ratio insufficient
A
Insufficient flow length ratio is caused by the high viscosity of CEF; high temperature, high pressure and large gate are the key
Injection Molding CEF injectionflow length ratiomelt viscosityinjection temperatureflow aid
Q
CEF extrusion film longitudinal streaks
Q
CEF film blocking and difficult delamination
Q
CEF extrusion profile bending deformation
A
Profile bending is caused by uneven cooling and uneven flow velocity; homogenization and alignment are the key to solving it
Extrusion & Post CEF extrusionbending deformationuniform coolinguniform flow velocitysizing sleeve
Q
CEF injection flash severe
A
Flash is caused by high-pressure injection and mold gap; reducing pressure and improving mold fitting are the key
Injection Molding CEF injectionflashclamping forceparting lineinjection pressure
Q
CEF extrusion film thickness uniformity poor
A
Film thickness uniformity needs to be synergistically optimized from three aspects: die design, gap adjustment and cooling
Extrusion & Post CEF filmthickness uniformitydie designextrusion swellair ring cooling
Q
CEF film thermal shrinkage rate too large
A
Film thermal shrinkage is caused by orientation freezing; reducing the draw ratio and annealing treatment are the key
Extrusion & Post CEF filmthermal shrinkageorientation releaseannealing treatmentbiaxial stretching
Q
CEF extrusion dimensional instability
A
Extrusion dimensional stability depends on feeding accuracy, temperature control and haul-off synchronization
Extrusion & Post CEF extrusiondimensional stabilityfeeding controltemperature PIDhaul-off synchronization