ASA Flow Mark Ripples
문제 현상
【Problem Phenomenon】Wavy flow marks on ASA product surface, uneven gloss
원인 분석
The melt front cold film breaks to form flow marks; low mold temperature and too slow injection speed causing the front to cool too fast are the main causes; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based only on experience
해결 방법
Increase mold temperature and melt temperature; increase injection speed; enlarge runner and gate to reduce front cooling; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
핵심 요약
ASA flow marks are the front condensation signal, raising temperature and speed improves; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!