ASA Flow Mark Ripples
Sorun Belirtisi
【Problem Phenomenon】Wavy flow marks on ASA product surface, uneven gloss
Neden Analizi
The melt front cold film breaks to form flow marks; low mold temperature and too slow injection speed causing the front to cool too fast are the main causes; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based only on experience
Çözüm
Increase mold temperature and melt temperature; increase injection speed; enlarge runner and gate to reduce front cooling; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Temel Çıkarım
ASA flow marks are the front condensation signal, raising temperature and speed improves; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!