Molds & Tooling
4 조회수
ASA Uneven Gloss
문제 현상
【Problem Phenomenon】Regional gloss differences on ASA product surface, high-gloss parts unqualified
원인 분석
Uneven mold temperature and cavity surface state differences cause different replication degrees; ASA surface finish is sensitive to mold temperature, differences immediately show as gloss difference; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based only on experience
해결 방법
Mold temperature homogenized and at upper limit; cavity polishing consistency check; venting optimization to prevent local air trap; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
핵심 요약
ASA gloss difference first check mold temperature uniformity, cavity polishing follows; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!