메뉴
재료 기계
인사이트
기사 동영상 문제 및 해결책
About
Chembull 소개 미디어 파트너
문의하기
언어
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
문제 및 해결책으로 돌아가기
Injection Molding 5 조회수

COC Flash

문제 현상
COC products have thin sheet flash at parting line and ejector pins, transparent parts flash affects optical appearance, residual marks obvious after trimming.
원인 분석
When injection pressure is too high or clamping force insufficient, melt squeezes into the parting line gap; COC injection specific pressure can reach 500~1100bar, high clamping requirement; mold wear gap expansion aggravates flash.
해결 방법
①Calculate clamping force to match high-pressure injection; ②parting line lapping to restore fit; ③optimize injection pressure curve, reduce speed and pressure at filling end; ④check hot runner valve pin sealing state.
핵심 요약
COC high-pressure injection process has high requirements on clamping and mold precision; flash treatment first checks hardware gap then adjusts process; transparent part flash should take mold repair as the ultimate solution.
COC; flash; clamping force; parting line; injection pressure; trimming

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다

ChemAI