Injection Molding 8 مشاهدة

COC Flash

ظاهرة المشكلة
COC products have thin sheet flash at parting line and ejector pins, transparent parts flash affects optical appearance, residual marks obvious after trimming.
تحليل الأسباب
When injection pressure is too high or clamping force insufficient, melt squeezes into the parting line gap; COC injection specific pressure can reach 500~1100bar, high clamping requirement; mold wear gap expansion aggravates flash.
الحل
①Calculate clamping force to match high-pressure injection; ②parting line lapping to restore fit; ③optimize injection pressure curve, reduce speed and pressure at filling end; ④check hot runner valve pin sealing state.
الخلاصة الأساسية
COC high-pressure injection process has high requirements on clamping and mold precision; flash treatment first checks hardware gap then adjusts process; transparent part flash should take mold repair as the ultimate solution.
COC; flash; clamping force; parting line; injection pressure; trimming