Processing Machinery 4 조회수

LDPE Film Low-temperature Brittleness

문제 현상
Film used in cold environments shows brittle cracking.
원인 분석
Although LDPE has good low-temperature toughness, low-temperature performance decreases when the formulation contains much filler or regrind; insufficient thickness also aggravates brittle cracking.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
해결 방법
①Select a cold-resistant formulation; ②Control the filler and regrind ratio; ③Ensure design thickness; ④Conduct low-temperature testing for verification.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
핵심 요약
Low-temperature applications require dedicated verification; formulation and thickness are the two elements of cold-resistant design.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
LDPE; film; low temperature; brittle cracking; formulation; cold resistance