Processing Machinery 7 visualizações

LDPE Film Low-temperature Brittleness

Fenómeno do problema
Film used in cold environments shows brittle cracking.
Análise das causas
Although LDPE has good low-temperature toughness, low-temperature performance decreases when the formulation contains much filler or regrind; insufficient thickness also aggravates brittle cracking.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Solução
①Select a cold-resistant formulation; ②Control the filler and regrind ratio; ③Ensure design thickness; ④Conduct low-temperature testing for verification.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Conclusão principal
Low-temperature applications require dedicated verification; formulation and thickness are the two elements of cold-resistant design.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
LDPE; film; low temperature; brittle cracking; formulation; cold resistance