메뉴
재료 기계
인사이트
기사 동영상 문제 및 해결책
About
Chembull 소개 미디어 파트너
문의하기
언어
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
문제 및 해결책으로 돌아가기
Extrusion & Post 4 조회수

LDPE Film Sharkskin

문제 현상
Periodic ripples like sharkskin appear on the film bubble surface, and the gloss of transparent film is lost
원인 분석
Melt fracture is a manifestation of extrusion shear stress exceeding the critical value; die temperature too low or resin melt index too low both trigger it; the elastic melt of LDPE long branched chains is sensitive to this
해결 방법
① Raise the die temperature by 10-20℃; ② switch to high melt index resin; ③ add fluorinated elastomer processing aid PPA; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
핵심 요약
The essence of sharkskin is the shear critical; the three routes of raising die temperature, changing melt index, and adding PPA are selected according to cost; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
LDPE;sharkskin;melt fracture;die temperature;PPA