Extrusion & Post 4 조회수

LLDPE printing adhesion

문제 현상
Poor ink adhesion on LLDPE film
원인 분석
Low surface energy and slip agent migration; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
해결 방법
Corona in place; PE-specific ink; migration check; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
핵심 요약
Printing relies on corona and ink matching; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
LLDPEprintingadhesionink