Extrusion & Post
5 görüntüleme
LLDPE printing adhesion
Sorun Belirtisi
Poor ink adhesion on LLDPE film
Neden Analizi
Low surface energy and slip agent migration; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Çözüm
Corona in place; PE-specific ink; migration check; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Temel Çıkarım
Printing relies on corona and ink matching; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu