PA12 Shrinkage Depression and Wall Thickness Upper Limit
문제 현상
【Problem phenomenon】PA12 thick-wall products had surface depressions and internal voids, with poor compensation effect
원인 분석
Insufficient product density, gas contained in the melt, excessively thick wall, and large thermal shrinkage jointly cause depressions; nylon process essentials clearly state that product thickness should not exceed 7-10mm
해결 방법
Control wall thickness within 7-10mm, reduce material and add ribs in thick areas; increase the melt amount, raise injection pressure, and extend injection time; fully dry and vent; lower barrel and mold temperature
핵심 요약
For thick-wall depressions, first reduce material; the 7-10mm wall thickness upper limit is a design red line; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!